Typical Magnetic Properties of Compression Bonded NdFeB Magnets
Grade1 | Br Remanence |
Hcb Coercive Force |
Hcj IntrinsicCoercivity |
Maximum Energy Product (BH)max |
Application |
DX-N4 | 400¡«500mT | 240¡«360kA/m | 640¡«800kA/m | 29¡«48kJ/m3 | Holder Stationary |
4000¡«5000Gs | 3000¡«4500 Oe | 8000¡«10000 Oe | 3.6¡«6.0MGOe | ||
DX-N6 | 600¡«700mT | 360¡«440kA/m | 640¡«800kA/m | 48¡«64kJ/m3 | Holder Micro-motor |
6000¡«7000Gs | 4500¡«5500 Oe | 8000¡«10000 Oe | 6.0¡«8.0MGOe | ||
DX-N8 | 600¡«700mT | 400¡«480kA/m | 640¡«800kA/m | 60¡«72kJ/m3 | |
6000¡«7000Gs | 5000¡«6000 Oe | 8000¡«11000 Oe | 7.5¡«9.0MGOe | ||
DX-N8H | 560¡«650mT | 400¡«480kA/m | 960¡«1200kA/m | 60¡«72kJ/m3 | |
5600¡«6500Gs | 5000¡«6000 Oe | 12000¡«15000 Oe | 7.5¡«9.0MGOe | ||
DX-N10 | 650¡«750mT | 400¡«480kA/m | 640¡«800kA/m | 72¡«88kJ/m3 | |
6500¡«7500Gs | 5000¡«6000 Oe | 8000¡«10000 Oe | 9.0¡«11.0MGOe | ||
DX-N12 | 650¡«750mT | 400¡«480kA/m | 640¡«800kA/m | 80¡«96kJ/m3 | |
6500¡«7500Gs | 5000¡«6000 Oe | 8000¡«10000 Oe | 10.0¡«12.0MGOe |
Typical Physical Characteristics of Compression Bonded NdFeB Magnets
Grade | Density | Hardness HRB |
Temperature Coefficient |
curie Temperature |
Max Operation Temperature |
Saturated Magnetic Field |
Thickness Of Coating |
Unit | g/cm3 | HRB | %/¡æ | ¡æ | ¡æ | kA/m | ¦Ìm |
DX-N4 | 6.0¡«6.5 | 40¡«45 | -0.11 | ¡Ý350 | 160 | 1600 | 5¡«30 |
DX-N6 | 6.0¡«6.2 | 40¡«45 | -0.11 | ¡Ý350 | 160 | 1600 | 5¡«30 |
DX-N8 | 6.0¡«6.2 | 35¡«38 | -0.11 | ¡Ý350 | 160 | 1600 | 5¡«30 |
DX-N8H | 6.0¡«6.2 | 35¡«38 | -0.12 | ¡Ý300 | 160 | 2400 | 5¡«30 |
DX-N10 | 6.0¡«6.2 | 35¡«38 | -0.10 | ¡Ý350 | 160 | 1600 | 5¡«30 |
DX-N12 | 6.1¡«6.4 | 35¡«38 | -0.10 | ¡Ý350 | 160 | 1600 | 5¡«30 |
Note: The coating material can be chosen according to customer's demand.